Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of YUHWA POLYPRO SB9108H - PP - Korea Petrochemical Ind. Co., Ltd

Material Data Center offers the following functions for YUHWA POLYPRO SB9108H:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Yuhwa Polypro datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Indice di fluidità a caldo, MFI 10 g/10min ASTM D 1238
Ritiro di stampaggio, parallelo 0.016 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ASTM Data
Resistenza alla trazione di snervamento 29.4 MPa ASTM D 638
Allungamento a rottura 200 % ASTM D 638
Modulo a flessione 1472 MPa ASTM D 790
Durezza Rockwell R 97 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 98 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 29 J/m ASTM D 256
Temperatura -20 °C -
Proprietà TermicheValoreUnitáNorma del test
ASTM Data
UL 94 combustibilitá HB - UL 94
Temperatura di fusione 168 °C ASTM D 3418
Temp.di rammollimento Vicat 152 °C ASTM D 1525
Altre ProprietàValoreUnitáNorma del test
Densità 910 kg/m³ ASTM D 792
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Caratteristiche speciali
Alto urto o modificato all'urto
Caratteristiche
Copolimero
Certifications
Contatto con gli alimenti, Approvato per l'utilizzo per contatto con alimenti secondo la FDA 21 CFR
Applicazioni
Automotive, Elettrotecnica ed electrici
Disponibilità geografica
Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.